UPDATE 1-Stress, corrosion caused 2018 Enbridge gas pipeline blast - Canadian agency

Thu, 05th Mar 2020 15:17

(Adds stress factor, interview with investigator)

By Rod Nickel

WINNIPEG, Manitoba, March 4 (Reuters) - An explosion and
fire in 2018 along an Enbridge Inc natural gas pipeline
in northern British Columbia was caused by normal stress that,
coupled with corrosion, created cracks, Canada's Transportation
Safety Board (TSB) said on Wednesday.

The pipeline operated by Enbridge subsidiary Westcoast
Energy Inc ruptured on Oct. 9, 2018, in a forested area near
Prince George. No one was injured, but the blast led to the
evacuation of 125 people, including from the Lheidli T'enneh
First Nation.

Police photos from a helicopter showed a nine-meter-deep
crater and dozens of scorched evergreen trees at the site.

The temporary shutdown of the line, which carries gas
destined for the Pacific Northwest, led to disruptions for
refineries owned by Royal Dutch Shell and Phillips 66
in the U.S. state of Washington.

The TSB said in a report that polyethylene tape used to
protect the pipeline's surface had deteriorated, allowing
moisture underneath and corrosion to develop. Stress on the
pipeline that was caused by normal operations, combined with the
corrosion, created the cracks, in a phenomenon known as "stress
corrosion cracking," said TSB senior investigator Jennifer
Philopoulos.

The board, an independent agency that reports to Parliament,
said it had investigated three other ruptures since 2002 with a
similar cause, all on TC Energy lines.

That section of line was last inspected 10 years before the
blast, and was scheduled for inspection the week the incident
occurred, said Michele Harradence, Enbridge's senior
vice-president of gas transmission and midstream.

"These are very stressful things to occur in your community
and we apologize for that," Harradence said in an interview from
Houston, Texas.

Enbridge has since begun integrity assessments of all its
gas pipelines in North America, adopted newer tools to detect
problems, expanded inspection criteria and increased scheduled
excavations to examine pipelines, she said.

The Canada Energy Regulator did not lay charges against
Enbridge.
(Reporting by Rod Nickel in Winnipeg, Manitoba; Editing by
Matthew Lewis and Grant McCool)

More News
7 Jan 2022 08:17

LONDON BRIEFING: Shell warns on cash outflows but continues buybacks

LONDON BRIEFING: Shell warns on cash outflows but continues buybacks

Read more
7 Jan 2022 07:57

LONDON MARKET PRE-OPEN: Shell says buybacks to continue "at pace"

LONDON MARKET PRE-OPEN: Shell says buybacks to continue "at pace"

Read more
7 Jan 2022 07:49

Shell to proceed with share buyback 'at pace' despite weaker oil performance

(Sharecast News) - Royal Dutch Shell said its $7bn share buyback programme would continue "at pace" despite weaker oil product sales due to the Omicron Covid variant and forex headwinds in Turkey.

Read more
7 Jan 2022 07:27

UPDATE 3-Shell pursues $7 billion buyback 'at pace' despite LNG troubles

* LNG production hit by outages in Australia* Marketing earnings impacted by Omicron slowdown (Adds share price)By Ron BoussoLONDON, Jan 7 (Reuters) - Royal Dutch Shell said it will pursue "at pace" a $7 billion share buyback largely funded from t...

Read more
7 Jan 2022 07:27

UPDATE 1-Shell to continue $7 bln buyback programme 'at pace'

(Adds detail)By Ron BoussoLONDON, Jan 7 (Reuters) - Royal Dutch Shell said on Friday its $7 billion share buyback programme, of which $1.5 billion has been completed, will continue "at pace" despite a slowdown in fuel demand due to the Omicron COV...

Read more
7 Jan 2022 07:27

UPDATE 2-Shell pursues $7 billion buyback 'at pace' despite LNG troubles

* LNG production hit by outages in Australia* Marketing earnings impacted by Omicron slowdown (Adds details, graphics)By Ron BoussoLONDON, Jan 7 (Reuters) - Royal Dutch Shell said it will pursue its $7 billion share buyback programme after selling ...

Read more
7 Jan 2022 07:10

Shell to continue $7 bln buyback programme 'at pace'

LONDON, Jan 7 (Reuters) - Royal Dutch Shell said on Friday its $7 billion share buyback programme, of which $1.5 billion has been completed, will continue "at pace" despite a slowdown in fuel demand due to the Omicron COVID-19 variant.(Reporting b...

Read more
6 Jan 2022 23:48

U.S. court rejects laundromat owners' bid to block sale of Texas oil refinery to Mexico's Pemex

By Stefanie EschenbacherHOUSTON/MEXICO CITY, Jan 6 (Reuters) - A U.S. court on Thursday tossed out a request from two laundromat owners to block Mexican state oil company Petroleos Mexicanos (Pemex) from acquiring majority control of a Texas oil r...

Read more
6 Jan 2022 12:16

UPDATE 2-Key Kazakh oil fields pump despite protests

(Updates with Shell, details, background)By Ron Bousso and Rowena EdwardsLONDON, Jan 6 (Reuters) - Oil production at Kazakhstan's top three fields is continuing even as some contractors gathered outside the largest Tengiz field in support of protes...

Read more
6 Jan 2022 12:00

Shell-backed U.S. solar developer raises $775 million in equity

By Nichola GroomJan 6 (Reuters) - Silicon Ranch Corp, the U.S. solar project developer backed by Royal Dutch Shell, on Thursday said it raised $775 million in equity capital from new and existing investors.The announcement comes as renewable energ...

Read more
5 Jan 2022 09:54

UPDATE 2-Commodity-linked stocks lift UK's FTSE 100 after dull start

(For a Reuters live blog on U.S., UK and European stock markets, click LIVE/ or type LIVE/ in a news window)* Ocado, LSEG, Ferguson gain as brokerages raise share ratings* Gains in oil majors offset risk-off sentiment* FTSE 100 up 0.2%, FTSE 250 of...

Read more
4 Jan 2022 17:00

LONDON MARKET CLOSE: Stocks start 2022 in style as airlines fly higher

LONDON MARKET CLOSE: Stocks start 2022 in style as airlines fly higher

Read more
4 Jan 2022 12:04

LONDON MARKET MIDDAY: Bright start to 2022 as travel stocks take off

LONDON MARKET MIDDAY: Bright start to 2022 as travel stocks take off

Read more
3 Jan 2022 13:26

U.S. refiner HollyFrontier warns of lower than expected throughput

Jan 3 (Reuters) - U.S. oil refiner HollyFrontier Corp's fourth-quarter throughput will be lower than forecast, hit by weather and turnaround setbacks at refineries in Washington, New Mexico and Oklahoma, the company warned on Monday.Flooding in B...

Read more
31 Dec 2021 13:08

LONDON MARKET CLOSE: Muted finish as FTSE 100 rallies 14% in 2021

LONDON MARKET CLOSE: Muted finish as FTSE 100 rallies 14% in 2021

Read more

Login to your account

Don't have an account? Click here to register.

Quickpicks are a member only feature

Login to your account

Don't have an account? Click here to register.