UPDATE 1-Stress, corrosion caused 2018 Enbridge gas pipeline blast - Canadian agency

Thu, 05th Mar 2020 15:17

(Adds stress factor, interview with investigator)

By Rod Nickel

WINNIPEG, Manitoba, March 4 (Reuters) - An explosion and
fire in 2018 along an Enbridge Inc natural gas pipeline
in northern British Columbia was caused by normal stress that,
coupled with corrosion, created cracks, Canada's Transportation
Safety Board (TSB) said on Wednesday.

The pipeline operated by Enbridge subsidiary Westcoast
Energy Inc ruptured on Oct. 9, 2018, in a forested area near
Prince George. No one was injured, but the blast led to the
evacuation of 125 people, including from the Lheidli T'enneh
First Nation.

Police photos from a helicopter showed a nine-meter-deep
crater and dozens of scorched evergreen trees at the site.

The temporary shutdown of the line, which carries gas
destined for the Pacific Northwest, led to disruptions for
refineries owned by Royal Dutch Shell and Phillips 66
in the U.S. state of Washington.

The TSB said in a report that polyethylene tape used to
protect the pipeline's surface had deteriorated, allowing
moisture underneath and corrosion to develop. Stress on the
pipeline that was caused by normal operations, combined with the
corrosion, created the cracks, in a phenomenon known as "stress
corrosion cracking," said TSB senior investigator Jennifer
Philopoulos.

The board, an independent agency that reports to Parliament,
said it had investigated three other ruptures since 2002 with a
similar cause, all on TC Energy lines.

That section of line was last inspected 10 years before the
blast, and was scheduled for inspection the week the incident
occurred, said Michele Harradence, Enbridge's senior
vice-president of gas transmission and midstream.

"These are very stressful things to occur in your community
and we apologize for that," Harradence said in an interview from
Houston, Texas.

Enbridge has since begun integrity assessments of all its
gas pipelines in North America, adopted newer tools to detect
problems, expanded inspection criteria and increased scheduled
excavations to examine pipelines, she said.

The Canada Energy Regulator did not lay charges against
Enbridge.
(Reporting by Rod Nickel in Winnipeg, Manitoba; Editing by
Matthew Lewis and Grant McCool)

More News
17 Nov 2021 16:02

UPDATE 3-Chevron, Exxon are among top spenders at Biden offshore auction

(Recasts, adds industry and environmentalist comments, details from sale, Biden FTC letter)By Nichola GroomNov 17 (Reuters) - U.S. oil majors Exxon Mobil Corp and Chevron Corp were among the top buyers at a federal auction of oil leases in the U.S...

Read more
17 Nov 2021 14:52

EXECUTIVE CHANGES: Deliveroo adds Flutter CEO to board; new Quarto CEO

EXECUTIVE CHANGES: Deliveroo adds Flutter CEO to board; new Quarto CEO

Read more
17 Nov 2021 10:07

UPDATE 1-LNG industry launches 'carbon neutral’ framework

(Adds context, rics to wider audience)By Susanna Twidale and Marwa RashadLONDON, Nov 17 (Reuters) - An international liquefied natural gas (LNG) body on Wednesday launched a framework for rules to declare cargoes carbon neutral as it seeks to make ...

Read more
17 Nov 2021 08:01

Russia's Rosneft acquires Shell's 37.5% stake in German refinery PCK Schwedt

MOSCOW, Nov 17 (Reuters) - Russian oil giant Rosneft has acquired Shell's 37.5% stake in German refinery PCK Schwedt, it said on Wednesday, exercising an option to buy and taking its shareholding to 91.67%.Italy's Eni holds a 8.33% stake in the re...

Read more
15 Nov 2021 18:56

North American natgas traders form company to better process trades

Nov 15 (Reuters) - A group of North American natural gas trading firms said on Monday they formed a new company called Eleox to manage post-trade processes more efficiently.The firms include units of BP PLC, Castleton Commodities International LLC...

Read more
15 Nov 2021 18:22

North Sea Crude-Forties steady, Brent diff edges lower

LONDON, Nov 15 (Reuters) - The North Sea Forties crude differential held steady on Monday while Brent slipped after two deals.* Royal Dutch Shell said on Monday it would scrap its dual share structure and move its head office to Britain from the ...

Read more
15 Nov 2021 17:10

LONDON MARKET CLOSE: Miners weigh on FTSE 100; Shell simplifies

LONDON MARKET CLOSE: Miners weigh on FTSE 100; Shell simplifies

Read more
15 Nov 2021 13:41

Shell shake-up leaves Dutch royally hacked off

By Toby SterlingAMSTERDAM, Nov 15 (Reuters) - Royal Dutch Shell's decision https://www.reuters.com/world/uk/shell-proposes-single-share-structure-tax-residence-uk-2021-11-15 to move its corporate headquarters and tax base to London may win over sha...

Read more
15 Nov 2021 12:37

GLOBAL MARKETS-Upbeat China data bolsters sentiment, oil tumbles

* China data lifts sentiment, boosts Aussie dollar* Sentiment in Europe tempered by rising COVID infections* Oil prices down more than 1%* Graphic: Global asset performance http://tmsnrt.rs/2yaDPgn* Graphic: World FX rates http://tmsnrt.rs/2egbfVh (...

Read more
15 Nov 2021 12:16

Shell to move head office to the UK, drop dual share structure

(Sharecast News) - Royal Dutch Shell is to overhaul its complex corporate structure, including shifting its headquarters to the UK and changing its name.

Read more
15 Nov 2021 12:04

LONDON MARKET MIDDAY: Caution sets in ahead of UK inflation, jobs data

LONDON MARKET MIDDAY: Caution sets in ahead of UK inflation, jobs data

Read more
15 Nov 2021 11:05

TOP NEWS SUMMARY: Shell simplifies; BBVA and Heineken buy

TOP NEWS SUMMARY: Shell simplifies; BBVA and Heineken buy

Read more
15 Nov 2021 10:43

UPDATE 2-European stocks clock fresh record highs; miners slide

* STOXX 600, DAX, CAC 40 hit record highs* Airbus boosts French stocks* BBVA drags down Spanish benchmark index (Adds comments, updates prices throughout)By Anisha Sircar and Shreyashi SanyalNov 15 (Reuters) - European shares hit another record peak...

Read more
15 Nov 2021 10:07

UPDATE 2-Cineworld, CMC markets help UK midcaps outperform bluechip FTSE 100

(For a Reuters live blog on U.S., UK and European stock markets, click LIVE/ or type LIVE/ in a news window)* Shell climbs on plans for single-share structure* CMC soars on plans to split into two* Cineworld jumps on box office revenue recovery* FTS...

Read more
15 Nov 2021 09:37

UPDATE 1-Dutch government 'unpleasantly surprised' by Shell HQ move to Britain

(Updates with details of Dutch tax issues)AMSTERDAM, Nov 15 (Reuters) - The Dutch government said on Monday it was "unpleasantly surprised" by news that Royal Dutch Shell PLC is planning to move its headquarters to London from The Hague."The Cabin...

Read more

Login to your account

Don't have an account? Click here to register.

Quickpicks are a member only feature

Login to your account

Don't have an account? Click here to register.